PLA-LW instructions
Most Teflon tube printers cannot run for a long time above 250°C. Long-term printing above this temperature may cause blockages. If the temperature exceeds 250°C, high-temperature printers such as metal hoses are required for printing.
2. If the bottom plate adhesion is not good when foaming, you can set the bottom valve and skirt when printing to improve the adhesion of the model bottom plate.
3. Yellowing of printed parts after high temperature foaming is a normal phenomenon, which can be alleviated by lowering the printing process.
4. As the PLA-LW foams continuously in the melting chamber of the high-temperature nozzle, the retraction basically does not work. It is normal to print the drawing during the time and space. It is recommended to print the vase model airplane drawings to reduce the influence of the drawing on the model.
The foaming ratio is related to temperature, printing speed, and nozzle melting cavity size. Pay attention to comparing the model design wall thickness according to your own printing situation, and adjust the extrusion rate, temperature, speed and other parameters.
The spool may be black