Feature

●Heat Resistance: Up to 750°C
●Heat resistant plaster for non-ferrous metal molding, can also be used for other glass casting such as zinc alloy, aluminum alloy, copper alloy, etc.
●Water content is 46~50% agitating time 4-6 minutes.


Description

The ratio of lime and water (amount of water mixture) is 46% to 50%. Water Consumption: Water weight / lime weight x 100% Example: When mixed with 46% lime and 22.0 lbs (10 kg) of lime: 10 kg x 46 / 100 = 4.6 L; Characteristic value (reference) Mixing Time: 46 - 50% Agitation Time: 6 minutes, Nure Compression Strength: 3.60 MPa Deformation Expansion Value: 0% % % Time: 50 - 60 minutes, Maximum Drying Temperature: 440 - 60 °F (200 - 280 °C), Casted Molding Temperature: 200 °C or higher.